⚠ Development preview: content and design are not final.

PA6 / PA66 compounds

GRN-PA6-C510

Brand GRN
GREENPOLYMER compound
Base resin PA6
PA6
Focus C
Carbon-fiber reinforced
Tier 5
Flame-retardant tier
Sequence 10
Development sequence 10

Flame-retardant carbon-fiber-reinforced PA6 (CFRPA)

Example grade / typical values — to be corrected by GREENPOLYMER

IllustrationFlammability ratingUL 94

A flame is applied as specified; afterflame time and whether drips ignite the cotton below decide the class

Description

Suitable parts

  • Joint arms
  • Battery compartment structures
  • Printing platform brackets

Light and stiff, flame retardant.

Key features

  • Light and stiff
  • Flame retardant

Applications

  • Robotics
  • Low-altitude aircraft
  • 3D printer structural parts

Parameters

Example grade / typical values — to be corrected by GREENPOLYMER

PropertyTypical valueTest standard
An illustration, not a measurement: Immersion method: weighed in air, then in a liquid; buoyancy gives the density 1.25–1.35 g/cm³ISO 1183
An illustration, not a measurement: A dumbbell specimen is pulled at a constant speed and the stress–strain curve is recorded until it breaksdry 160–220 MPaISO 527-1/-2
An illustration, not a measurement: A pendulum breaks a notched bar supported at both ends; the energy it absorbs gives the result23 °C; dry 6–10 kJ/m²ISO 179-1/1eA
An illustration, not a measurement: A loaded bar is heated in an oil bath at a steady rate; the result is the temperature at which it reaches the set deflection1.80 MPa 190–210 °CISO 75-1/-2
An illustration, not a measurement: A flame is applied as specified; afterflame time and whether drips ignite the cotton below decide the class1.5 mm; design target, subject to test report V-0UL 94
An illustration, not a measurement: Three-point bending: the bar rests on two supports and is loaded in the middle; the initial slope gives the modulus 12–18 GPaISO 178

Typical values. Refer to the actual TDS. Values are typical industry ranges for this material class, not GREENPOLYMER test data; to be corrected by GREENPOLYMER. Flammability rating, CTI, light transmittance and weathering: design target, subject to test report (for each grade).

IllustrationISO 1183

Immersion method: weighed in air, then in a liquid; buoyancy gives the density

Contact us

Tell us about the part, material requirements, equipment and expected volume. We will recommend suitable grades and the validation data you need.