⚠ Development preview: content and design are not final.

PC/ABS compounds

GB5105

Prefix GB
Alloy / blend (non-flame-retardant)
Series 5
PC/ABS
Filler 1
Glass fiber
Filler content 05
5 %

5 % glass-fiber-reinforced PC/ABS

  1. Planned grade
  2. Available
  3. GREENPOLYMER TDS
  • HBUL 94
  • 107–121 °CHDT · 1.80 MPa

Datasheet

Each value is shown with its test standard and conditions.

  • Glass-fiber content—5%
  • DensityISO 11831.17–1.20g/cm³
  • Tensile modulusISO 527-1/-22.3–4.8GPa
  • Heat deflection temperatureISO 75-1/-2 · 1.80 MPa107–121°C

Typical values; not for use as specifications.

Processing window

  • Drying95–110 °C, 4 h, desiccant dryer
  • Mold temperature70–90 °C
  • Melt temperature230–275 °C (usually 270 °C)
  • ≤ 0.02 %Max. moisture before processing
  • 0.25–0.45 % (in flow) / 0.35–0.55 % (across flow)Molding shrinkage

Contact us