PC/ABS compounds

GB5125

Prefix GB
Alloy / blend (non-flame-retardant)
Series 5
PC/ABS
Filler 1
Glass fiber
Filler content 25
25 %

25 % glass-fiber-reinforced PC/ABS

  1. Planned grade
  2. Available
  3. GREENPOLYMER TDS
  • HBUL 94
  • 119–126 °CHDT · 1.80 MPa

Datasheet

Each value is shown with its test standard and conditions.

  • Glass-fiber content—25%
  • DensityISO 11831.31–1.34g/cm³
  • Tensile modulusISO 527-1/-27.2–10GPa
  • Izod notched impact strengthISO 180/1A · 23 °C8–12kJ/m²
  • Heat deflection temperatureISO 75-1/-2 · 1.80 MPa119–126°C

Typical values; not for use as specifications.

Processing window

  • Drying95–110 °C, 4 h, desiccant dryer
  • Mold temperature70–90 °C
  • Melt temperature230–275 °C (usually 270 °C)
  • ≤ 0.02 %Max. moisture before processing
  • 0.15–0.40 % (in flow) / 0.30–0.50 % (across flow)Molding shrinkage