PC/ABS compounds

GB5115

Prefix GB
Alloy / blend (non-flame-retardant)
Series 5
PC/ABS
Filler 1
Glass fiber
Filler content 15
15 %

15 % glass-fiber-reinforced PC/ABS

  1. Planned grade
  2. Available
  3. GREENPOLYMER TDS
  • HBUL 94
  • 119–121 °CHDT · 1.80 MPa

Datasheet

Each value is shown with its test standard and conditions.

  • Glass-fiber content—15%
  • DensityISO 11831.24–1.27g/cm³
  • Tensile modulusISO 527-1/-24.8–7.2GPa
  • Izod notched impact strengthISO 180/1A · 23 °C≈ 8kJ/m²
  • Heat deflection temperatureISO 75-1/-2 · 1.80 MPa119–121°C

Typical values; not for use as specifications.

Processing window

  • Drying95–110 °C, 4 h, desiccant dryer
  • Mold temperature70–90 °C
  • Melt temperature230–275 °C (usually 270 °C)
  • ≤ 0.02 %Max. moisture before processing
  • 0.2–0.4 % (flow) / 0.3–0.5 % (transverse)Molding shrinkage